dc.title | Zn2SnO4 nanowires versus nanoplates: Electrochemical performance and morphological evolution during Li-cycling | |
dc.contributor.author | Cherian, C.T. | |
dc.contributor.author | Zheng, M. | |
dc.contributor.author | Reddy, M.V. | |
dc.contributor.author | Chowdari, B.V.R. | |
dc.contributor.author | Sow, C.H. | |
dc.date.accessioned | 2014-10-16T09:49:23Z | |
dc.date.available | 2014-10-16T09:49:23Z | |
dc.date.issued | 2013-07-10 | |
dc.identifier.citation | Cherian, C.T., Zheng, M., Reddy, M.V., Chowdari, B.V.R., Sow, C.H. (2013-07-10). Zn2SnO4 nanowires versus nanoplates: Electrochemical performance and morphological evolution during Li-cycling. ACS Applied Materials and Interfaces 5 (13) : 6054-6060. ScholarBank@NUS Repository. https://doi.org/10.1021/am400802j | |
dc.identifier.issn | 19448244 | |
dc.identifier.uri | http://scholarbank.nus.edu.sg/handle/10635/98618 | |
dc.description.abstract | Zn2SnO4 nanowires have been synthesized directly on stainless steel substrate without any buffer layers by the vapor transport method. The structural and morphological properties are investigated by means of X-ray diffraction (XRD) and transmission electron microscopy (TEM). The electrochemical performance of Zn2SnO4 nanowires is examined by galvanostatic cycling and cyclic voltammetry (CV) measurements in two different voltage windows, 0.005-3 and 0.005-1.5 V vs Li and compared to that of Zn2SnO4 nanoplates prepared by hydrothermal method. Galvanostatic cycling studies of Zn2SnO4 nanowires in the voltage range 0.005-3 V, at a current of 120 mA g-1, show a reversible capacity of 1000 (±5) mAh g-1 with almost stable capacity for first 10 cycles, which thereafter fades to 695 mAh g-1 by 60 cycles. Upon cycling in the voltage range 0.005-1.5 V vs Li, a stable, reversible capacity of 680 (±5) mAh g-1 is observed for first 10 cycles with a capacity retention of 58% between 10-50 cycles. On the other hand, Zn2SnO4 nanoplates show drastic capacity fading up to 10 cycles and then showed a capacity retention of 80% and 70% between 10 and 50 cycles when cycled in the voltage range 0.005-1.5 and 0.005-3 V, respectively. The structural and morphological evolutions during cycling and their implications on the Li-cycling behavior of Zn2SnO4 nanowires are examined. The effect of the choice of voltage range and initial morphology of the active material on the Li-cycleabilty is also elucidated. © 2013 American Chemical Society. | |
dc.description.uri | http://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1021/am400802j | |
dc.source | Scopus | |
dc.subject | anodes | |
dc.subject | Li-cycling | |
dc.subject | lithium ion batteries | |
dc.subject | morphological dependence | |
dc.subject | Zn2SnO4 nanoplates | |
dc.subject | Zn2SnO4 nanowires | |
dc.type | Article | |
dc.contributor.department | PHYSICS | |
dc.description.doi | 10.1021/am400802j | |
dc.description.sourcetitle | ACS Applied Materials and Interfaces | |
dc.description.volume | 5 | |
dc.description.issue | 13 | |
dc.description.page | 6054-6060 | |
dc.identifier.isiut | 000321810000025 | |
Appears in Collections: | Staff Publications |
Show simple item record
Files in This Item:
There are no files associated with this item.
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.