dc.titleCasting solvent effects on morphologies, gas transport properties of a novel 6FDA/PMDA-TMMDA copolyimide membrane and its derived carbon membranes
dc.contributor.authorShao, L.
dc.contributor.authorChung, T.-S.
dc.contributor.authorWensley, G.
dc.contributor.authorGoh, S.H.
dc.contributor.authorPramoda, K.P.
dc.date.accessioned2014-10-09T06:44:20Z
dc.date.available2014-10-09T06:44:20Z
dc.date.issued2004-11-15
dc.identifier.citationShao, L., Chung, T.-S., Wensley, G., Goh, S.H., Pramoda, K.P. (2004-11-15). Casting solvent effects on morphologies, gas transport properties of a novel 6FDA/PMDA-TMMDA copolyimide membrane and its derived carbon membranes. Journal of Membrane Science 244 (1-2) : 77-87. ScholarBank@NUS Repository. https://doi.org/10.1016/j.memsci.2004.07.005
dc.identifier.issn03767388
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/88617
dc.description.abstractWe have observed that solvents play an important role on the membrane morphology and gas separation performance of a novel 6FDA/PMDA-TMMDA copolyimide [copoly(4,4'-methylenebis(2,6-dimethyl)-2,2-bis(3,4-dicarboxylphenyl) hexafluoro propane/pyromellitic) diimide]. Copolyimide films cast from CH 2Cl 2 or NMP (1-methyl-2-pyrrolidinone) show amorphous morphology, while films cast from DMF (N,N-dimethylformamide) have crystalline structure which has been confirmed by polarized microscope, XRD and gas sorption tests. Gas transport properties of different morphological films are significantly different. Furthermore, we also report that gas separation performance of carbon molecular sieve membranes (CMSMs) pyrolyzed from different morphological precursors is strongly dependent on pyrolysis temperatures. Results show that the permeability of CMSMs at different pyrolysis temperatures follows the order: 550°C > 650°C > 800°C and the separation factor is in the order: 800°C > 650°C > 550°C. The differences between CMSMs derived from different morphological precursors decrease with an increase in pyrolysis temperatures. At low pyrolysis temperature, the CMSMs' structure and separation performance could significantly be affected by the decomposition temperature of the precursor, however, at higher pyrolysis temperatures, the dominant factor for the CMSMs' structure and performance is the pyrolysis temperature due to the complete degradation of the polymeric precursor. © 2004 Elsevier B.V. All rights reserved.
dc.description.urihttp://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1016/j.memsci.2004.07.005
dc.sourceScopus
dc.subjectCarbon molecular sieve membranes (CMSMs)
dc.subjectCrystalline structure
dc.subjectFluoropolyimides
dc.subjectGas separation
dc.subjectSolvent effect
dc.typeArticle
dc.contributor.departmentCHEMISTRY
dc.contributor.departmentCHEMICAL & BIOMOLECULAR ENGINEERING
dc.description.doi10.1016/j.memsci.2004.07.005
dc.description.sourcetitleJournal of Membrane Science
dc.description.volume244
dc.description.issue1-2
dc.description.page77-87
dc.description.codenJMESD
dc.identifier.isiut000225232300008
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.