dc.titleEnhancing tensile and compressive strength of magnesium using ball milled Al+CNT reinforcement
dc.contributor.authorHabibi, M.K.
dc.contributor.authorHamouda, A.M.S.
dc.contributor.authorGupta, M.
dc.date.accessioned2014-06-17T06:20:17Z
dc.date.available2014-06-17T06:20:17Z
dc.date.issued2012-01-18
dc.identifier.citationHabibi, M.K., Hamouda, A.M.S., Gupta, M. (2012-01-18). Enhancing tensile and compressive strength of magnesium using ball milled Al+CNT reinforcement. Composites Science and Technology 72 (2) : 290-298. ScholarBank@NUS Repository. https://doi.org/10.1016/j.compscitech.2011.11.015
dc.identifier.issn02663538
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/60190
dc.description.abstractIn this work, Mg/Al-CNT nano-composites were fabricated using powder metallurgy route involving microwave assisted rapid sintering and hot extrusion. Ball milled Al-CNT particles comprising different contents of CNTs coated with fixed amount of Al were used for strengthening. Microstructural characterization of these Mg/Al-CNT nano-composites reveal reasonably uniform distribution of Al-CNT particles up to CNT content of 0.30% by weight, significant grain refinement and the presence of minimal porosity compared to monolithic Mg. Importantly, for the nominally identical processing conditions, the textures of as-extruded nano-composite specimens is significantly influenced by the presence of Al-CNT particles. Nano-composite configurations exhibit different tensile and compressive response as a function of CNT content. Among the different Mg/Al-CNT formulations synthesized, the Mg/Al-CNT configuration with Al-CNT particles composition of 1.00% Al and 0.30% CNT by weight (Mg/1.00Al-0.30CNT) exhibit higher tensile yield strength (0.2% YS), ultimate tensile strength (UTS) and failure strain (FS) (up to +72%, +48%, +9%, respectively) compared to monolithic Mg.In terms of compressive response, it exhibits the best overall compressive properties compared to the monolithic Mg with an improvement of 63% in the compressive yield strength (0.2% CYS) and 80% in ultimate compressive strength (UCS), but failure strain was compromised. © 2011 Elsevier Ltd.
dc.description.urihttp://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1016/j.compscitech.2011.11.015
dc.sourceScopus
dc.subjectA. Metal-matrix composites (MMCs)
dc.subjectA. Nano-composite
dc.subjectB. Mechanical properties
dc.subjectE. Microwave processing
dc.typeArticle
dc.contributor.departmentMECHANICAL ENGINEERING
dc.description.doi10.1016/j.compscitech.2011.11.015
dc.description.sourcetitleComposites Science and Technology
dc.description.volume72
dc.description.issue2
dc.description.page290-298
dc.description.codenCSTCE
dc.identifier.isiut000300648000022
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.