Please use this identifier to cite or link to this item: https://doi.org/10.1016/S0142-9418(01)00068-X
DC FieldValue
dc.titleEnhanced resistance of polyurethane sealants against cohesive failure under prolonged combination of water and heat
dc.contributor.authorChew, M.Y.L.
dc.contributor.authorZhou, X.
dc.date.accessioned2013-10-14T04:37:08Z
dc.date.available2013-10-14T04:37:08Z
dc.date.issued2002
dc.identifier.citationChew, M.Y.L., Zhou, X. (2002). Enhanced resistance of polyurethane sealants against cohesive failure under prolonged combination of water and heat. Polymer Testing 21 (2) : 187-193. ScholarBank@NUS Repository. https://doi.org/10.1016/S0142-9418(01)00068-X
dc.identifier.issn01429418
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/45660
dc.description.abstractThe enhanced resistance of polyurethane (PU) sealants against cohesive failure under prolonged combination of water and heat was analyzed. The specimens of multi-component sealant was cured for 14 days and single-component were cured for 21 days. The elastic recovery of PU sealant was recorded at 100% after the same immersion period and a slight increase of 2% was observed.
dc.description.urihttp://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1016/S0142-9418(01)00068-X
dc.sourceScopus
dc.subjectCohesive failure
dc.subjectDurability
dc.subjectHot water resistance
dc.subjectPolyurethane
dc.subjectSealant
dc.subjectTropics
dc.typeArticle
dc.contributor.departmentBUILDING
dc.description.doi10.1016/S0142-9418(01)00068-X
dc.description.sourcetitlePolymer Testing
dc.description.volume21
dc.description.issue2
dc.description.page187-193
dc.description.codenPOTED
dc.identifier.isiut000173005300014
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.