dc.titleInvestigation of the electrochemical breakdown response in sensitised aa5083 aluminium alloy
dc.contributor.authorLiew, YanHan
dc.contributor.authorWijesinghe, Sudesh
dc.contributor.authorBlackwood, Daniel J.
dc.date.accessioned2022-10-12T08:04:49Z
dc.date.available2022-10-12T08:04:49Z
dc.date.issued2021-06-30
dc.identifier.citationLiew, YanHan, Wijesinghe, Sudesh, Blackwood, Daniel J. (2021-06-30). Investigation of the electrochemical breakdown response in sensitised aa5083 aluminium alloy. Sustainability (Switzerland) 13 (13) : 7342. ScholarBank@NUS Repository. https://doi.org/10.3390/su13137342
dc.identifier.issn2071-1050
dc.identifier.urihttps://scholarbank.nus.edu.sg/handle/10635/232441
dc.description.abstractThe light-weight aluminium alloys play an important role in reducing emissions from the transport industry. However, to take full advantage of these, the corrosion mechanisms that govern their failure need to be properly understood. Hence, the electrochemical response, especially after passive film breakdown, of the aluminium alloy AA5083 was analysed via potentiodynamic polarisation. By starting the scans at the relatively negative potential of ?1.4 V (vs. SCE), the reduction of water in the electrolyte causes a localised increase in pH, leading to a preferential attack on the susceptible regions in the (sensitised) microstructure; that is, the deleterious ?-Al3Mg2 along the grain boundaries. Subsequently, in the later stages of the potentiodynamic scan, these regions that have been degraded by the dissolution of ?-Al3Mg2 undergo imperfect repassivation, leading them to be vulnerable to localised breakdowns. These conditions allowed for the discovery of a discernible trend after breakdown, in which AA5083 microstructures with a more extensive ?-Al3Mg2 region (both in size and in amount) recorded a more rapid increase in the measured current density. In particular, the potential at which the anodic current density reached 1 × 10?4 A cm?2 was correlated with the extent of ?-Al3Mg2 formed during isothermal heat-treatments. This work provides a possible pathway towards the development of an electrochemical quantification technique for the extent of ?-Al3Mg2 growth, degree of sensitisation, and, ultimately, the intergranular corrosion (IGC) susceptibility of the microstructure of AA5083 components used in industrial applications. © 2021 by the authors. Licensee MDPI, Basel, Switzerland.
dc.publisherMDPI
dc.rightsAttribution 4.0 International
dc.rights.urihttps://creativecommons.org/licenses/by/4.0/
dc.sourceScopus OA2021
dc.subjectAluminium alloy 5083
dc.subjectPotentiodynamic polarisation
dc.subjectSensitisation
dc.subject?-Al3Mg2
dc.typeArticle
dc.contributor.departmentCOLLEGE OF DESIGN AND ENGINEERING
dc.description.doi10.3390/su13137342
dc.description.sourcetitleSustainability (Switzerland)
dc.description.volume13
dc.description.issue13
dc.description.page7342
Appears in Collections:Staff Publications
Elements

Show simple item record
Files in This Item:
File Description SizeFormatAccess SettingsVersion 
10_3390_su13137342.pdf2.53 MBAdobe PDF

OPEN

NoneView/Download

Google ScholarTM

Check

Altmetric


This item is licensed under a Creative Commons License Creative Commons