dc.titleInfluence of micron-Ti and Nano-Cu additions on the microstructure and mechanical properties of pure magnesium
dc.contributor.authorSeetharaman S.
dc.contributor.authorSubramanian J.
dc.contributor.authorGupta M.
dc.contributor.authorHamouda A.S.
dc.date.accessioned2020-09-08T03:22:02Z
dc.date.available2020-09-08T03:22:02Z
dc.date.issued2012
dc.identifier.citationSeetharaman S., Subramanian J., Gupta M., Hamouda A.S. (2012). Influence of micron-Ti and Nano-Cu additions on the microstructure and mechanical properties of pure magnesium. Metals 2 (3) : 274-291. ScholarBank@NUS Repository. https://doi.org/10.3390/met2030274
dc.identifier.issn2075-4701
dc.identifier.urihttps://scholarbank.nus.edu.sg/handle/10635/174591
dc.description.abstractn this study, metallic elements that have limited/negligible solubility in pure magnesium (Mg) were incorporated in Mg using the disintegrated melt deposition technique. The metallic elements added include: (i) micron sized titanium (Ti) particulates with negligible solubility; (ii) nano sized copper (Cu) particulates with limited solubility; and (iii) the combination of micro-Ti and nano-Cu. The combined metallic addition (Ti + Cu) was carried out with and without preprocessing by ball-milling. The microstructure and mechanical properties of the developed Mg-materials were investigated. Microstructure observation revealed grain refinement due to the individual and combined presence of hard metallic particulates. The mechanical properties evaluation revealed a significant improvement in microhardness, tensile and compressive strengths. Individual additions of Ti and Cu resulted in Mg-Ti composite and Mg-Cu alloy respectively, and their mechanical properties were influenced by the inherent properties of the particulates and the resulting second phases, if any. In the case of combined addition, the significant improvement in properties were observed in Mg-(Ti + Cu)BM composite containing ball milled (Ti + Cu) particulates, when compared to direct addition of Ti and Cu particulates. The change in particle morphology, formation of Ti3Cu intermetallic and good interfacial bonding with the matrix achieved due to preprocessing, contributed to its superior strength and ductility, in case of Mg-(Ti + Cu)BM composite. The best combination of hardness, tensile and compressive behavior was exhibited by Mg-(Ti + Cu)BM composite formulation. © 2012 by the authors; licensee MDPI, Basel, Switzerland.
dc.sourceUnpaywall 20200831
dc.typeArticle
dc.contributor.departmentMECHANICAL ENGINEERING
dc.description.doi10.3390/met2030274
dc.description.sourcetitleMetals
dc.description.volume2
dc.description.issue3
dc.description.page274-291
dc.published.statePublished
Appears in Collections:Staff Publications
Elements

Show simple item record
Files in This Item:
File Description SizeFormatAccess SettingsVersion 
10_3390_met2030274.pdf1.31 MBAdobe PDF

OPEN

PublishedView/Download

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.