Please use this identifier to cite or link to this item: https://doi.org/10.1109/IITC.2011.5940290
DC FieldValue
dc.titleNanoindentation for quality control of ULK films
dc.contributor.authorYeap, K.B.
dc.contributor.authorZeng, K.
dc.contributor.authorHangen, U.
dc.contributor.authorZschech, E.
dc.date.accessioned2014-10-07T09:15:07Z
dc.date.available2014-10-07T09:15:07Z
dc.date.issued2011
dc.identifier.citationYeap, K.B.,Zeng, K.,Hangen, U.,Zschech, E. (2011). Nanoindentation for quality control of ULK films. 2011 IEEE International Interconnect Technology Conference and 2011 Materials for Advanced Metallization, IITC/MAM 2011 : -. ScholarBank@NUS Repository. <a href="https://doi.org/10.1109/IITC.2011.5940290" target="_blank">https://doi.org/10.1109/IITC.2011.5940290</a>
dc.identifier.isbn9781457705038
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/86034
dc.description.abstractThe structural integrity of ultra low-k (ULK) dielectrics is highly dependent on their mechanical properties, e.g. fracture toughness, adhesion and elastic modulus. For materials and process development, the ULK interfacial adhesion can be determined applying four-point-bending (FPB) and double-cantilever-beam (DCB) methods in out-of-fab labs. On the other hand, the characterization of interfacial adhesion is also very important for process control and quality assurance in-line/at-line. The ability to detect a defective ULK films at an early processing step could potentially save processing and material cost. Therefore, the development of the current experimental methodology for the purpose of in-line/at-line mechanical properties evaluation is of great interest for semiconductor industry and tool suppliers. In this paper, a wedge indentation method particularly suitable for ULK quality control is described. The indentation experiment can be conducted on an as-deposited ULK film, without further sample preparation. Furthermore, a simple analysis and a straight forward experimental methodology are introduced, allowing a short time-to-data. Interfacial delaminations of the ULK films are observed after the wedge indenter has been penetrated into the film at a critical penetration depth. The indentation stress that induced the interfacial delamination ( o) was found to be proportional to the indentation volumetric strain. Therefore, assuming that the energy release rate is equivalent to the interfacial adhesion, the interfacial adhesion of the ULK films is given as =(1f 2)to 2/2Ef. The interfacial adhesion values as concluded from this analysis have been validated through a sufficient number of indentation experiments on several ULK materials and film thicknesses. In addition to the wedge indentation experiment, several independent simulation studies and four-point-bending experiments have shown consistent interfacial adhesion values, compared to the results from the analysis mentioned above. The wedge indentation method developed in this study has a strong potential for semiconductor industry application, especially as a quality control technique. © 2011 IEEE.
dc.description.urihttp://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1109/IITC.2011.5940290
dc.sourceScopus
dc.typeConference Paper
dc.contributor.departmentMECHANICAL ENGINEERING
dc.description.doi10.1109/IITC.2011.5940290
dc.description.sourcetitle2011 IEEE International Interconnect Technology Conference and 2011 Materials for Advanced Metallization, IITC/MAM 2011
dc.description.page-
dc.identifier.isiutNOT_IN_WOS
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.