Please use this identifier to cite or link to this item: https://scholarbank.nus.edu.sg/handle/10635/60024
DC FieldValue
dc.titleEDM performance of TiC/copper-based sintered electrodes
dc.contributor.authorLi, L.
dc.contributor.authorWong, Y.S.
dc.contributor.authorFuh, J.Y.H.
dc.contributor.authorLu, L.
dc.date.accessioned2014-06-17T06:18:20Z
dc.date.available2014-06-17T06:18:20Z
dc.date.issued2001-12
dc.identifier.citationLi, L.,Wong, Y.S.,Fuh, J.Y.H.,Lu, L. (2001-12). EDM performance of TiC/copper-based sintered electrodes. Materials and Design 22 (8) : 669-678. ScholarBank@NUS Repository.
dc.identifier.issn02613069
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/60024
dc.description.abstractThis paper presents a study of the effect of titanium carbide (TiC) on the performance of sintered copper-based materials as electrical discharge machining (EDM) electrodes. The aim of this study was to provide a preliminary evaluation of EDM electrodes fabricated by laser-based sintering using rapid prototyping technology (RP). Six batches of titanium carbide with content from 5% to 45% were fabricated by mixing, ball milling, pressing, and liquid phase sintering with copper-tungsten (Cu-W) and copper (Cu), respectively. The performance of the newly formed material is compared with commercial electrodes. The densification of TiC/Cu-W system was improved by the addition of nickel (Ni), as Ni shows good solubility in both Cu and W. The distribution of particle size becomes narrow as the proportion of TiC is increased. A uniform dispersion of small TiC particles in the Cu-W system and a narrow particle size distribution provide the possibility of obtaining dense electrodes. With increasing TiC, the relative density first increased and then decreased, whereas the electrical resistivity first decreased and then increased. EDM electrodes, with the addition of TiC, show good performance in surface finishing. This is an important characteristic as RP-sintered EDM electrodes are expected to be used as finishing electrodes. The surface roughness of most specimens is less than those machined using commercial electrodes. Electrodes with 15% TiC show the highest relative density, lowest electrical resistivity, and good EDM performance, i.e. lowest tool wear ratio (TWR) and highest material removal rate (MRR) at low current, and the best surface finish not only at low current, but also at high current. © 2001 Elsevier Science Ltd. All rights reserved.
dc.sourceScopus
dc.subjectElectrical discharge machining (EDM)
dc.subjectLiquid phase sintering
dc.subjectRapid prototyping (RP)
dc.typeArticle
dc.contributor.departmentMECHANICAL ENGINEERING
dc.description.sourcetitleMaterials and Design
dc.description.volume22
dc.description.issue8
dc.description.page669-678
dc.identifier.isiutNOT_IN_WOS
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.