Please use this identifier to cite or link to this item: https://doi.org/10.1016/j.msea.2011.10.081
DC FieldValue
dc.titleThe role of aluminum oxide particulate reinforcements on cyclic fatigue and final fracture behavior of a novel magnesium alloy
dc.contributor.authorSrivatsan, T.S.
dc.contributor.authorGodbole, C.
dc.contributor.authorParamsothy, M.
dc.contributor.authorGupta, M.
dc.date.accessioned2014-10-07T09:12:02Z
dc.date.available2014-10-07T09:12:02Z
dc.date.issued2012-01-15
dc.identifier.citationSrivatsan, T.S., Godbole, C., Paramsothy, M., Gupta, M. (2012-01-15). The role of aluminum oxide particulate reinforcements on cyclic fatigue and final fracture behavior of a novel magnesium alloy. Materials Science and Engineering A 532 : 196-211. ScholarBank@NUS Repository. https://doi.org/10.1016/j.msea.2011.10.081
dc.identifier.issn09215093
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/85777
dc.description.abstractIn this research paper, the microstructure, hardness, tensile properties, tensile fracture, cyclic stress amplitude fatigue response and final fracture behavior of a novel magnesium alloy, denoted as AZ(12)1, discontinuously reinforced with nano-particulates of aluminum oxide (Al 2O 3) is neatly presented and convincingly discussed. The matrix alloy, which had three weight percent more aluminum than the monolithic counterpart (AZ91), was produced by solidification processing followed by hot extrusion. Properties spanning microhardness, tensile, high cycle fatigue and fracture behavior of the discontinuously reinforced magnesium alloy (AZ(12)1) are compared with the unreinforced monolithic alloy (AZ91). The elastic modulus, yield strength, tensile strength of the reinforced magnesium alloy is marginally higher than the unreinforced counterpart. The ductility quantified by elongation to failure over 0.5in. (12.7mm) gage length of the test specimen and reduction in specimen cross-section area of the composite was noticeably lower than the monolithic counterpart. At the fine microscopic level both tensile fracture and cyclic fatigue fracture of the composite revealed fewer features reminiscent of the occurrence of locally ductile mechanisms when compared with the monolithic counterpart. Over a range of maximum stress and at two different load ratios the cyclic fatigue resistance of the composite was noticeably inferior to the monolithic counterpart. The key mechanisms responsible for the inferior cyclic fatigue life and fracture resistance of the composite microstructure are elucidated. © 2011 Elsevier B.V.
dc.description.urihttp://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1016/j.msea.2011.10.081
dc.sourceScopus
dc.subjectAluminum oxide
dc.subjectCyclic fatigue
dc.subjectFracture
dc.subjectMagnesium alloy
dc.subjectNano-size
dc.subjectParticulate reinforcements
dc.typeArticle
dc.contributor.departmentMECHANICAL ENGINEERING
dc.description.doi10.1016/j.msea.2011.10.081
dc.description.sourcetitleMaterials Science and Engineering A
dc.description.volume532
dc.description.page196-211
dc.identifier.isiut000301160100028
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.