dc.titleTwo-stage sintering of nano-sized yttria stabilized zirconia process by powder injection moulding
dc.contributor.authorYu, P.C.
dc.contributor.authorLi, Q.F.
dc.contributor.authorFuh, J.Y.H.
dc.contributor.authorLi, T.
dc.contributor.authorLu, L.
dc.date.accessioned2014-06-17T06:37:31Z
dc.date.available2014-06-17T06:37:31Z
dc.date.issued2007-10-01
dc.identifier.citationYu, P.C., Li, Q.F., Fuh, J.Y.H., Li, T., Lu, L. (2007-10-01). Two-stage sintering of nano-sized yttria stabilized zirconia process by powder injection moulding. Journal of Materials Processing Technology 192-193 : 312-318. ScholarBank@NUS Repository. https://doi.org/10.1016/j.jmatprotec.2007.04.097
dc.identifier.issn09240136
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/61636
dc.description.abstractPowder injection moulding (PIM) is capable of mass producing intricately shaped components. In recent years, this technology has been adopted in the electronic, computer, chemical and medical industries. The 3 mol% yttria stabilized zirconia (Y-TZP) is well recognised for its high fracture toughness. PIM of nano-sized Y-TZP hence offer attractive potential applications. Grain growth however is a major problem for nano-sized powder. Initial researches proposed that high green density and minimum sintering temperature are beneficial in controlling the grain growth of nano-sized powder. In view of the constraint of low green density of PIM samples, grain growth control will be even challenging. Two-stage sintering (2SS) is reported to be able to refine the microstructure and enhance the material properties. This method simply modifies the sintering route by firing the sample at high temperature follow by rapidly cooling down and dwelling at lower temperature. The objective of this work is to monitor the effect of 2SS on the nano-sized Y-TZP process by PIM. Dimensional changes, weight loss, density, hardness as well as microstructure are study after the sintering and compare to the conventional isothermal sintering. The process condition at 1350 °C follow by 900 °C is found to be able to achieve comparable hardness as isothermal sintering at 1500 °C. With a finer microstructure, 2SS can potentially improve the grain size dependant material properties of nano-Y-TZP in the near future. © 2007 Elsevier B.V. All rights reserved.
dc.description.urihttp://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1016/j.jmatprotec.2007.04.097
dc.sourceScopus
dc.subjectGrain growth
dc.subjectNano-sized Y-TZP
dc.subjectPowder injection moulding
dc.subjectTwo-stage sintering
dc.typeArticle
dc.contributor.departmentMECHANICAL ENGINEERING
dc.description.doi10.1016/j.jmatprotec.2007.04.097
dc.description.sourcetitleJournal of Materials Processing Technology
dc.description.volume192-193
dc.description.page312-318
dc.description.codenJMPTE
dc.identifier.isiut000249314100048
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.