Title: Growth of mullite whiskers in mechanochemically activated oxides doped with WO3
Authors: Kong, L.B. 
Huang, H.
Zhang, T.S.
Ma, J.
Boey, F.
Zhang, R.F.
Wang, Z.H.
Keywords: Anisotropy
Grain growth
Milling
Mullite
Whiskers
Issue Date: Dec-2003
Citation: Kong, L.B., Huang, H., Zhang, T.S., Ma, J., Boey, F., Zhang, R.F., Wang, Z.H. (2003-12). Growth of mullite whiskers in mechanochemically activated oxides doped with WO3. Journal of the European Ceramic Society 23 (13) : 2257-2264. ScholarBank@NUS Repository. https://doi.org/10.1016/S0955-2219(03)00083-9
Abstract: The effect of WO3 on mullite formation and mullite whisker morphology, in oxide mixtures activated by a high-energy ball milling process, was investigated. Differential thermal analysis (DTA) measurement indicated that WO3 enhanced the mullite phase formation, with mullitization temperature of 951 °C, 921 °C and 835 °C for the samples doped with 5, 10 and 20 mol% WO3, respectively. However, the presence of WO3 had an undesired effect on the whisker morphology. A decrease in the length of mullite whisker was observed with increasing WO3 content. The effect of WO3 on the mullite phase formation temperature, as well as the whisker morphology, was explained using a dissolution-precipitation mechanism. © 2003 Elsevier Ltd. All rights reserved.
Source Title: Journal of the European Ceramic Society
URI: http://scholarbank.nus.edu.sg/handle/10635/111410
ISSN: 09552219
DOI: 10.1016/S0955-2219(03)00083-9
Appears in Collections:Staff Publications

Show full item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.