dc.titleSynthesis of lead zirconate titanate from an amorphous precursor by mechanical activation
dc.contributor.authorJunmin, X.
dc.contributor.authorWang, J.
dc.contributor.authorWeiseng, T.
dc.date.accessioned2014-10-29T08:41:13Z
dc.date.available2014-10-29T08:41:13Z
dc.date.issued2000-08-10
dc.identifier.citationJunmin, X., Wang, J., Weiseng, T. (2000-08-10). Synthesis of lead zirconate titanate from an amorphous precursor by mechanical activation. Journal of Alloys and Compounds 308 (1-2) : 139-146. ScholarBank@NUS Repository. https://doi.org/10.1016/S0925-8388(00)00917-8
dc.identifier.issn09258388
dc.identifier.urihttp://scholarbank.nus.edu.sg/handle/10635/107227
dc.description.abstractMany of the chemistry-based processing routes for functional ceramics inevitably involve calcining the chemical-derived precursors at an intermediate/high temperature, in order to form the designed ceramic phase. This is very undesirable, although widely used, as the calcination can result in an extensive degree of crystal growth and particle coarsening at the calcination temperature and therefore ruins almost all the advantages offered by the chemistry-based processing routes, such as an ultrafine particle size and high sintering-reactivity. Using a specifically designed PZT precursor prepared by co-precipitation, it is demonstrated that the precursor-to-ceramic conversion can alternatively be realized by mechanical activation. In this connection, a single phase, nanocrystalline perovskite PZT powder has been successfully derived from an amorphous hydroxide precursor by mechanical activation. The resulting PZT powder was well dispersed, and the particle size was in the range of 30-50 nm, as observed using the scanning electron microscopy and transmission electron microscopy. This is in contrast to the poor particle characteristics, represented by very coarse and irregular particle and agglomerate sizes, for the powder derived from calcination at 750 °C. The activation-triggered PZT powder was sintered to a density of 97.6% theoretical density at 1150 °C for 1 h. Sintered PZT ceramic exhibits a dielectric constant of 927 at room temperature and a peak dielectric constant of approximately 9100 at the Curie point of 380 °C when measured at the frequency of 1 kHz.
dc.description.urihttp://libproxy1.nus.edu.sg/login?url=http://dx.doi.org/10.1016/S0925-8388(00)00917-8
dc.sourceScopus
dc.typeArticle
dc.contributor.departmentMATERIALS SCIENCE
dc.description.doi10.1016/S0925-8388(00)00917-8
dc.description.sourcetitleJournal of Alloys and Compounds
dc.description.volume308
dc.description.issue1-2
dc.description.page139-146
dc.description.codenJALCE
dc.identifier.isiut000089264600023
Appears in Collections:Staff Publications

Show simple item record
Files in This Item:
There are no files associated with this item.

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.